Re: [MW:13117] Inconel 625 to 70Cu-30Ni Alloy Dissimilar weld

Dear,

I think you should go for ERNiCu7/ENicu7 consumable. Special metal electrode performance is better than others.

Regards,
VJ

On Wed, Nov 30, 2011 at 3:04 PM, MUHAMMAD SHAHZAD <shehzadqc@gmail.com> wrote:

Dear Sir

I want to weld Inconel 625 (P No. 43) to 70Cu-30Ni alloy (P No.34) which welding Rod/Electrode is the most suitable for GTAW/SMAW process.

--
Muhammad Shahzad
Materials & Corrosion Engineer
Arabian Petrochemical Company (Petrochemya/Sabic)


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...