Wednesday, November 30, 2011

Re: [MW:13115] Minimum acceptance criteria for weld reinforcement for pipe and plate

jamil,

the weld reinforcement depends on the weld thickness and the same can be found in table 341.3.2 of B31.3.

On Wed, Nov 30, 2011 at 3:21 PM, md jamil ahmad <jamilmech2009@gmail.com> wrote:
Dear All,
          Any body explain me,1) what is the minimum acceptance criteria for out side weld reinforcement for power piping or process piping
          I think,in general 1.6 to 3mm,is it correct or not.
         2) In inside welding of pipe what is the minimum and maximum reinforcement criteria,please tell me as per ASME Code.


REGARD
JAMIL AHMAD
KSA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.