Wednesday, November 30, 2011

Re: [MW:13110] Radiographic technique shot

Dear Sir,
Thanks for your valued expert advice.
As per ASME SEC V  T-290, no where is mentioned about thickness wise as well as diameter wise only technique wise.
If i make only technique wise, is that any violation as per ASME SEC -V
Thanks
Pradip 

On Tue, Nov 29, 2011 at 10:42 PM, Raju Kandula <rgkandula@gmail.com> wrote:
Dear Pradip..
 
    technique as well as diameter and thickness is right..  the essential variables that has to be noted on the docimentation, changes corresponding to diff daiameter adn the thickness... like iqi selction and the no of films used and the location length, so it wil be easy and prefer to do documentation as per diamter and thickness so it is easy for some one to understand the documentation and easy to trace for future referance...
 
regards
raju kandula

On Tue, Nov 29, 2011 at 9:14 AM, pradip kumar sil <pradipsil@gmail.com> wrote:
Dear Experts,
As per ASME Sec. V T-290 shows radiographic technique documentation details needs only each technic wise i.e single wall/ double wall. But client demanded each technique wise as well as diametre & thickness wise.
My question is which one is correct either technique wise or technique as well as diametre & thicknesswise.
Thanks in advance.
Regards
Pradip

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...