RE: [MW:13103] what is the root cause for copper crack in saw welding ?

 Hi MPK,
 
 
It's a form of solidification cracking caused  due to localized segregation of low melting elements. Copper is one of the elements which tends to form so, for C.S and high strength and medium strength low alloy steels.
 
Please see the reference below.
 
Thanks.
 
P.Goswami,P.Eng,IWE
 
http://content.lincolnelectric.com/pdfs/knowledge/articles/content/weldcracking.pdf
 

Date: Tue, 29 Nov 2011 16:32:37 +0300
Subject: [MW:13100] what is the root cause for copper crack in saw welding ?
From: ranmi2007@gmail.com
To: materials-welding@googlegroups.com

Dear Experts,
What is the Root cause for copper crack in SAW welding ?

thanks,
MPK


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...