Re: [MW:13099] Gasket for Hydro testing of pressure vessel

Dear Ali,
We can use original service gaskets in locations other than reinstatement flanges @ test boundaries. For reinstatement flanges we can use any other because we will reinstate the original.

Muthusamy
UAE

On 28 November 2011 20:49, Aly <mhaskar.aly@gmail.com> wrote:
Dear Experts,
Could you please advise on whether to use original service gaskets for hydro testing or any other gasket ca be used?
 
Thanks in advance.
 
Mhaskar Aly
UAE

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...