Dear Mehdi,
For Density, as some friends mentioned before, you can use a densitometer. but about the contrast you have to keep in mind that in fact the contrast is not a quantitative factor. It is defined as "contrast is a difference between the density of two adjacent part of a film", so you can measure the density of two part of the film and the difference is related to the contrast. but please consider that transition in film density is usual, so measuring the contrast as a quantitative factor is not practical.
  Regards
On Tue, Nov 29, 2011 at 2:42 PM, Mohamed Motawea <eng.motawea@gmail.com> wrote:
Dear sir;
There is differnec between the film contrast and film density.
Regards;
Mohamed
On Nov 29, 10:43 am, yogeshkumar Kumbhar <kumbharyoge...@gmail.com>
wrote:
> Dear Mehdi,
>
> Measure radiography film contrast ( Density ) by densitometer.
>
> Regard's
>
> Yogesh V Kumbhar
>
>
>
> On Tue, Nov 29, 2011 at 10:21 AM, Mehdi Emami <mehdi.em...@yahoo.com> wrote:> > w.r.t. applicable code/standard/contract documents.- Hide quoted text -
> > Dear experts
> > Can anyone tell me how to measure contrast of radiographic films?in fact,
> > I want Definition & contrast calculation method
> > Thanks
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
>
> - Show quoted text -
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
M. Shokri Arfaei
International Welding Engineer (IWE)
ASNT NDT Level III
ERI Metallurgy Lab. Manager
Tel: +98-21-66282127
  Fax: +98-21-66282779
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments