Re: [MW:13088] 4130 pipe material

Vimal,

4130 material falls under A519 (standard specification for seamless carbon and alloy steel mechanical tubing)

Its a grade of A519 material.

On Tue, Nov 29, 2011 at 1:02 PM, Vimal Kumar <vimal.fajar@gmail.com> wrote:
Dear all, 

            May I know the expert advice on this
1. What is 4130 material
2. 4130 is under which specification
3. If 4130 is a general term for some group of material, what are the material that are called 4130

With regards

Vimal Kumar
+65 9100 2565

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...