Re: [MW:13084] QW-200.4

Dear Sir,
 
Thanks for reply, but apart from your expaination, please let me know can we combine two existing WPS of different processes (Say GTAW & SMAW) of less than 13 mm thk in a single production joint as per QW-200.1 (f) ?
On Sun, Nov 27, 2011 at 10:41 PM, Aly <mhaskar.aly@gmail.com> wrote:
Advantage of combining two processes:
 
Suppose u have two wps as below
 
1: WPS with GTAW with 13mm base plate thickness (Base metal Qualification range is 26mm max) 
 
2:WPS with SMAW with 20mm base plate thickness (Base metal Qualification range is 40mm max) 
 
If u combined these two WPS, the advantage you can get is u can weld GTAW process double the max thickness between two process ie  (2 x 20mm = 40mm) not upto 26mm only.
 
You can use more than one WPS in one single joint, just to increase base metal thickness qualification range one can combine two process as per QW-200.4(b).
 
You can create many WPS from one single PQR as needed.
 
Hope this is clear for you..
 
Mhaskar Aly
 
 
 
 
-------Original Message-------
 
Date: 18/11/2011 21:08:13
Subject: [MW:13020] QW-200.4
 

Dear experts....Can anyone provide some Section IX interpretations for clause no.QW-200.4 ?................Can anybody explain this clause better ?...........It clearly states that multiple wps of different processes can be combined together and we can make a single wps combining that processes...........and from one pqr combining different processes ,individual wps can be prepared for each process..............the root deposites clause of min 13 mm is an ALTERNATE requirement....is it really applicable in which situation ?...............

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards

Hiren Sevak
Surveyor
Bureau Veritas - Ahmedabad
207, Abhishree
Opp Star India Bazaar,
Satellite Road,
Ahmedabad-380015
Tel No. 079-26925491/92

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...