use optical emission spectrgraph for PMI and compare results with ASME sec II Part A or B.

Regards,
Abdul Hafeez

-----Original Message-----
From: c.nopadon@vipco-thai.com
Sent: 27/11/2011 4:38:25 am
Subject: RE: [MW:13064] Type of steel as per chemical proterties

Normal PMI equipment like XRF spectrometer cannot identify C. From my
knowledge , it must be portable spectrometer or similar which will be more
expensive than normal PMI. If PMI is required for stainless of which carbon
content is the issue such as 347H , it is possible that the client will
require PMI result with carbon content.

Regards,

C.Nopadon

From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of pankaj abhang
Sent: Saturday, November 26, 2011 1:04 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:13061] Type of steel as per chemical proterties

Dear How you identified carbon in PMI?..........


Regards,
pankaj

On Fri, Nov 4, 2011 at 11:50 PM, meisam shokri arfaei
<meisamshokri@gmail.com> wrote:

Dear friend,

This material is something like CK30. But this kind of material is heat
treatable and you have to sure about this. It is recommended to have a
metallographic test on it for undrestanding such a heat treatment.

Regards

On Fri, Nov 4, 2011 at 1:22 PM, U WYNN-NAING <u.wynn-naing@total.com> wrote:

Dear Experts,

We did PMI test on one unknown machine bolt from crane boom rest and result
is as follow:

Can someone tell me how can we trace the steel grade base on this result.

Is there any software available?

Thanks and Rgds,

WN

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
<mailto:materials-welding%2Bunsubscribe@googlegroups.com>
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--

M. Shokri Arfaei

International Welding Engineer (IWE)

ASNT NDT Level III

ERI Metallurgy Lab. Manager

Tel: +98-21-66283696

Fax: +98-21-66283693

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
<mailto:materials-welding%2Bunsubscribe@googlegroups.com>
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...