Dear Mr. Himan,

Normally, Inconels are higkly corrosion resistant alloys, which do not
need passivation. However, you are advised to show assemby drawing near
welded area which needs to be looked into.

S.N.Bagchi.
<snbagchi@aol.in>


-----Original Message-----
From: Himan Nikdin <himannikdin@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Sun, Nov 27, 2011 5:15 pm
Subject: [MW:13069] Inconel Passivation


Dear Friends


I have stone trap which will be made from API 5L-X52 that inner side
overlaied by Inconel, I want to know we shall clean welded separate
pipes welded area by acid pickling or any passivation is mandatory???


I will be appreciated if anybody can help me.


Thank you in advance.
Himan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...