Sunday, November 27, 2011

Re: [MW:13066] Welding of AISI 316L to A516 Gr B regarding

 
Also it needs PWHT, since it thickness is more than 19 mm (As per ASME)

 
T.Mahendran,
Tabouk - KSA,

 
--- On Sat, 11/26/11, george.dilintas@gr.bureauveritas.com <george.dilintas@gr.bureauveritas.com> wrote:

From: george.dilintas@gr.bureauveritas.com <george.dilintas@gr.bureauveritas.com>
Subject: Re: [MW:13063] Welding of AISI 316L to A516 Gr B regarding
To: "materials-welding" <materials-welding@googlegroups.com>
Date: Saturday, November 26, 2011, 1:08 PM

Just 309 is ok. 316 with carbon steel will give hot cracks because of low FN. You need a filler metal with much higher Cr and Ni content to avoid low FN
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager

  From: Eswaran samikannu [eswaranaws@yahoo.co.in]
  Sent: 26/11/2011 12:54 ZE5B
  To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
  Subject: [MW:13062] Welding of AISI 316L to A516 Gr B regarding


Good day to all,
Please refer the attachment  for joint configuration, I have to qualify the procedure for AISI 316L to A516 Gr B steel
Thickness of the job maximum 64 mm. I proposed to use 35 mm thickness plate for qualification.Code requirement ASME Sec IX
My plan as follows
1) Buttering the Bevel area of A516 Gr B material using E 309 consumables up to 3 to 5 mm
2) Machining of Bevel & PT (NDT) & Fit up
3) Welding of A516 Gr B to to AISI 316L using E316 consumables 

Kindly  advice me what preheat temperature  & Interpass temperature can maintained during welding, Any PWHT required or not,any other precautionary measures during welding & mechanical testing.
My client not specified anything. Please someone advice to me.
Thanks
Regards
E.Jegan  
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...