Re: [MW:13061] Type of steel as per chemical proterties

Dear How you identified carbon in PMI?..........


Regards,
pankaj

On Fri, Nov 4, 2011 at 11:50 PM, meisam shokri arfaei <meisamshokri@gmail.com> wrote:
Dear friend,
This material is something like CK30. But this kind of material is heat treatable and you have to sure about this. It is recommended to have a metallographic test on it for undrestanding such a heat treatment.
 
Regards

On Fri, Nov 4, 2011 at 1:22 PM, U WYNN-NAING <u.wynn-naing@total.com> wrote:

Dear Experts,

 

We did PMI test on one unknown machine bolt from crane boom rest and result is as follow:

Can someone tell me how can we trace the steel grade base on this result.

Is there any software available?

 

Thanks and Rgds,

 

WN

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
M. Shokri Arfaei
International Welding Engineer (IWE)
ASNT NDT Level III
ERI Metallurgy Lab. Manager
Tel: +98-21-66283696
Fax: +98-21-66283693

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...