Re: [MW:13048] Titanium

Dear Vinod,
 
Yes Titanium is sutable for -90 degree C. but it depends on application & Service line
case to case. Please find attached the titanium impact test was conducted at 4K or -269 degree C. & full Mechanicat & Fracture details are also mentioned for your reference,
 
Regards
Amit Pahuja
Sr. Welding Engineer
B-Tech (Welding),
IWE-IIW, CSWIP-3.1
NDT Level-II, RT,UT.PT.MT
BOIST-OFFSHORE CERTIFICATES.
 
QATAR

On Wed, Nov 23, 2011 at 11:48 AM, Vinod Kataria <vinod.kataria@blissanand.com> wrote:

Dear All,

Could you please advise if Titanium is suitable for -90 degree C if yes please provide some back up document.

Regards

Vinod

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...