Re: [MW:13044] PTC Requirement for S.S.

Dear Vijay

If welding is performed with the use of filler material up -196 deg C, Production Test Coupan is not required.
for PTC requirements refer UHA 51 h

Best Regards

Rajesh Patel
Executive Engineer  - Materials Technology, QA/QC & Standards





From:        Vijay Katkar <katkar.vijay22@gmail.com>
To:        materials-welding@googlegroups.com
Date:        23-11-11 21:44
Subject:        [MW:13040] PTC Requirement for S.S.
Sent by:        materials-welding@googlegroups.com




Dear All,
 
I have one vessel with M.D.M.T -140 Degree C. for base metal (SA 240 TP 304) impact test is exampted as per UHA 51 Of ASME section VIII Division- 1 but consumable and procedure qualification impact test is required as UHA-51 ,
PTC is required for vessel with above condition, please advice .........
 
 
Regards
 
Vijay Katkar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...