Friday, November 18, 2011

RE: [MW:13022] Subcontractor WPS

Hi,
 
If a contractual item call for a specific WPS then you shall use it , other wise the contractual item should specify the aplicable standard for weldings and you shall use it and choose or qualify a WPS according to that standard.

Note: Generally the contractor write the WPS as a basic engineering deliverable.
 

Date: Fri, 18 Nov 2011 15:02:40 +0530
Subject: [MW:13019] Subcontractor WPS
From: hirensevak80@gmail.com
To: materials-welding@googlegroups.com

Dear all, can anybody guide for following problem ?...................for example any EPC company has goven a contract for fabrication to a sub contractor....and that EPC company wants the contractor to follow their WPS only...and also they are forcing the contractor to conduct welder qualification tests only......my question is that can any contractor follow the WPS established by their client without further qualification from his side ?................

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...