Sunday, November 27, 2011

Răspuns: [MW:13072] RE: 13068] ADVANCED NDT

Dear friend,
Phased Array is in this moment unstandardized technique;but you can make indentification inspection with PA ,and after, evaluation with classical technical methodes-AVG and/or CAD;TOFD is special tecniques for  perpendicularly reflectors(this technique is in function of your capability);PA is new mode for the estimate of remanent life or materials(termomechanical steel for power plant for example)
Best regards
material and NDT inspector-met eng Iacob Catalin
 
De la: Pieper QSI <info@pieper-qsi.nl>
Către: materials-welding@googlegroups.com
Trimis: Duminică, 27 Noiembrie 2011 13:50:42
Subiect: [MW:13070] RE: 13068] ADVANCED NDT
Ultrasonic techniques like Phased Array and some older Time Of Flight Difference become more and more accepted / required for NDT examination. But in your case if you want to become an expert in NDT techniques you will need knowledge of all kind of NDT techniques in order to advise / execute a proper technology for finding the defects you’re looking for.
 
Met vriendelijke groeten / Best Regards
 
Herman Pieper
 
Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax:     +31 (0)84 7539225
Cell:     +31 (0)6 51691215
www.pieper-qsi.nl
 
Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens Mehdi Emami
Verzonden: zondag 27 november 2011 8:55
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:13068] ADVANCED NDT
 
Dear friends, dear experts
I want to become expert in one of the most advanced techniques NDT. What method or methods to suit the needs of industry today, do you recommend?
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...