[MW:13089] RE: 13083] Preheating temperature of 2nd process when use two welding process in one single joint (GTAW+SMAW)

Dear Mhaskar,

If you take that temperature before start welding SMAW process then it will be consider as preheating temperature for SMAW

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Aly
Sent: Tuesday, 29 November, 2011 2:40 AM
To: materials-welding@googlegroups.com
Subject: [MW:13083] Preheating temperature of 2nd process when use two welding process in one single joint (GTAW+SMAW)

 

Dear Experts,

 

When we are using two process (GTAW + SMAW) on pipe test coupon of a PQR, Root run & hot is done with GTAW process, immediately after hot pass we have started SMAW process,

 

Prior to start of SMAW process, temperature of coupon noted was 95 deg C

 

My question is whether this 95deg C will be considered as preheating temperature for SMAW process

 

Kindly advise in the light ASME Codes

 

Thanks in advance

 

Mhaskar Aly

UAE 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...