Dear All,
 
I have one vessel with M.D.M.T -140 Degree C. for base metal (SA 240 TP 304) impact test is exampted as per UHA 51 Of ASME section VIII Division- 1 but consumable and procedure qualification impact test is required as UHA-51 ,
PTC is required for vessel with above condition, please advice .........
 
 
Regards
 
Vijay Katkar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.