Friday, May 14, 2010

Re: [MW:5172] welding Repair percentage

Soliman,
 
You can calculate on the Total length welded based on the radiography. For eg the total length weld is 1meter and the repair length is say 50 mm. Then
 
50/1000 * 100 will give you the Repair percentage.

J.GERALD JAYAKUMAR
00919344954677
 


--- On Fri, 5/14/10, mohamed soliman <msoliman79@yahoo.com> wrote:

From: mohamed soliman <msoliman79@yahoo.com>
Subject: [MW:5170] welding Repair percentage
To: materials-welding@googlegroups.com
Date: Friday, May 14, 2010, 11:04 AM


 
Hi to all,
 
We are building new booster station ,our contractor wanted to calculate the repair percentage of the welding based on the linear lenght .Alwyas this should be calculated by the joint wise .Can any one refere any international standard that state how to calculate this rate.Please note that the client specs did not specify any thing on that.
 
Please send me your thoughts ASAP.
 
Regards
Soliman

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...