Dear Soliman,
% weld repair based on linear length will be calculated as follows: Total length (mm) of the weld radiographed against total length (mm) of repairs which will give you the % of repair in length wise. In this you need to calculate the length of each repair based on RT film.
The % of repair will be very low in length wise compared to joint wise. As you indicted, joint wise is more practical compared to length wise.
Regards,
L. Prabhu kumar,
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mohamed soliman
Sent: Friday, May 14, 2010 3:35 PM
To: materials-welding@googlegroups.com
Subject: [MW:5170] welding Repair percentage
Hi to all,
We are building new booster station ,our contractor wanted to calculate the repair percentage of the welding based on the linear lenght .Alwyas this should be calculated by the joint wise .Can any one refere any international standard that state how to calculate this rate.Please note that the client specs did not specify any thing on that.
Please send me your thoughts ASAP.
Regards
Soliman
|
------------------------------------------------------------------------------------------------------------------------------------------------------------------- DISCLAIMER: The information contained in this communication is intended solely for the use of the individual or entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged information. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If you have received this communication in error, please notify us immediately by responding to this email and then delete it from your system. Saipem India Projects Limited (SIPL) is neither liable for the proper and complete transmission of the information contained in this communication nor for any delay in its receipt. ------------------------------------------------------------------------------------------------------------------------------------------------------------------- |