Hi
Since the Cu element is unspecified element in the material spec. & it is not mandatory also. If it is present in the chemical analysis, just check Section II Part A SA 20 for limitations of unspecified elements. Based on that we can accept the material and MTC also.
ASOK KUMAR.P
QA / QC ENGINEER
ZAMIL STEEL - PED
EX: 6414
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of smruthi mohan
Sent: Sunday, April 18, 2010 5:00 PM
To: materials-welding@googlegroups.com
Subject: [MW:4854] Acceptability of MTC.
Hi.
Anybody please advise me on the below,
we have an 12" End Cap (SA403 WP316L)for an ASME job. But in test certificate there is an additional element content (Cu (0,370))is present in the chemical Analysis. please advice me that we can accept this item or not.
Thanks in advance.
SMRUTHI MOHAN
ENGINEER - MATERIALS.
QICL, FUJAIRAH
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment