Re: [MW:4853] RT TABLE

Dear Sanjeev,
 
AWS D1.1 nowhere required the % of RT this has to be identified by the Client, But in general in Clause 6.15 of AWS D1.1  page 219 these requirements are  in 3 classifications as 1.Full testing 2.Partial testing and 3 Spot testing.
 
Regards.
 
V.Ravishanker.


From: Sanjeev Gupta <sanjeev.gupta1968@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, 18 April, 2010 10:09:51 AM
Subject: [MW:4851] RT TABLE

Dear All,
 
Can anybody suggest  that  where in AWS D 1.1 it is mentioned the % RT to be taken.Pls mention or specify the exact clause number.(Like as mentioned in ASME B 31.3 Table No T 321.3)
 
Regards
Sanjeev
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...