hi, as per aASME section-VIII-UCS56,if the welded joint nominal thicknessthickness more than 38mm shall be PWHT. As per ASME Section-1,PW-39.Welded joint htickness more than 19mm shall be PWHT.Pls.Refer with the applicable code. Karthikeyan.S Getabec Energy Co.,Ltd. 379,Moo6,Soi8,Nikhomphatana, Rayong-21180, Thailand. Phone: 0066 38 897035-8 (Off) Fax: 0066 38 897034 Hand Phone: 0066 892512282 --- On Sat, 4/17/10, manpreet <manpreetsin88@rediffmail.com> wrote:
|
--