Re: [MW:4841] back gauging for fit up welds

In double or single  V joint configration without backing plates, if you weld from outside, gouging and grinding is required  up to the sound metal and to be filled with new weld to coform the soundness of the weld.
 
 
V.Ravishanker,


From: manpreet <manpreetsin88@rediffmail.com>
To: materials-welding@googlegroups.com
Sent: Fri, 16 April, 2010 7:29:13 AM
Subject: [MW:0] back gauging for fit up welds

Dear all

why do we need to do backgauging in fit up welds?

what other places ,it is required to do backgauging?

Which specification to be referred?


regards
Manpreet Singh
09867303228

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...