Dear all,
Usually purging is necessry to eliminate presence of oxygen while doing low alloy steels and SS materials,To eliminate oxides inside the pipe weld beads, Cofirm purging should  be with nitrogen  and mixture of hydrogen and nitrogen or organ well before the welding  to remove oxygen in side the pipe.
 
Ravishanker, 


From: qaqcmpm <mamujeebali@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Thu, 15 April, 2010 11:27:58 AM
Subject: [MW:4843] Ar purge for Low Alloy steel

One of our client specn asks for argon purging of root pass (pressure
retaining welds) for GTAW for Low alloy Cr-Mo steel? why it is
required any idea?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

To unsubscribe, reply using "remove me" as the subject.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...