Friday, April 9, 2010

Re: [MW:4759] Re: Film digitizer unit supplier and approximate cost


More details about scanning of X-ray films:

With our scanner, the film has to be slightly overexposed, i.e. optical density between 1.0 and 1.4. The scanner shall illuminate the film from both sides.  

Regards,

Claes Gillenius
Development Engineer, MMA. (Spec. stainless and non Fe-alloys)
Direct tel:  +46 (0)31 509315
Mobile +46 (0)707532012
Company                ESAB AB
Address                  Box 8004, 402 77  Gothenburg, Sweden
                                 Lindholmsallén 9
Company  reg number        556005-7738



Shashank Vagal <nach_sam@yahoo.com>
Sent by: materials-welding@googlegroups.com

2010-04-07 17:58

Please respond to
materials-welding@googlegroups.com

To
materials-welding@googlegroups.com
cc
Subject
Re: [MW:4743] Re: Film digitizer unit supplier and approximate cost





Thanks Claes,
The films are acceptable for most purposes. Now, please explain how you do it.
Rgds,
Shashank Vagal

--- On Wed, 7/4/10, claes.gillenius@esab.se <claes.gillenius@esab.se> wrote:


From: claes.gillenius@esab.se <claes.gillenius@esab.se>
Subject: Re: [MW:4738] Re: Film digitizer unit supplier and approximate cost
To: materials-welding@googlegroups.com
Date: Wednesday, 7 April, 2010, 4:11 PM


Please see attached jpeg-files. Scanned X-ray films. Ni-base weldment in 9% Ni-steel overhead position.





Best regards,



Claes Gillenius
Development Engineer, MMA. (Spec. stainless and non Fe-alloys)
Direct tel:  +46 (0)31 509315
Mobile +46 (0)707532012
Company                ESAB AB
Address                  Box 8004, 402 77  Gothenburg, Sweden
                                Lindholmsallén 9
Company  reg number        556005-7738




Shashank Vagal <nach_sam@yahoo.com>
Sent by: materials-welding@googlegroups.com

2010-04-07 12:16
Please respond to
materials-welding@googlegroups.com

To
materials-welding@googlegroups.com
cc
Subject
Re: [MW:4737] Re: Film digitizer unit supplier and approximate cost







Claes,
Could you please send across a few radiographs thus digitized and saved, for review?
Rgds,
Shashank Vagal

--- On Wed, 7/4/10, claes.gillenius@esab.se <claes.gillenius@esab.se> wrote:

From: claes.gillenius@esab.se <claes.gillenius@esab.se>
Subject: Re: [MW:4733] Re: Film digitizer unit supplier and approximate cost
To: materials-welding@googlegroups.com
Date: Wednesday, 7 April, 2010, 2:44 PM


We use our old system with traditional developed films. With the help of a ordinaryl cheap flat bed scanner we can make digital copies with acceptable quality.

Regards,



Claes Gillenius
Development Engineer, MMA. (Spec. stainless and non Fe-alloys)
Direct tel:  +46 (0)31 509315
Mobile +46 (0)707532012
Company                ESAB AB
Address                  Box 8004, 402 77  Gothenburg, Sweden
                               Lindholmsallén 9
Company  reg number        556005-7738




hpi001 <pieper-qsi@kpnmail.nl>
Sent by: materials-welding@googlegroups.com

2010-04-07 05:37

Please respond to
materials-welding@googlegroups.com

To
"Materials & Welding" <materials-welding@googlegroups.com>
cc
Subject
[MW:4727] Re: Film digitizer unit supplier and approximate cost









Dear Hrishi,

In Europe the company General Electric is a supplier of such systems.
Costs will be anywhere near to $45.000.
I will send some information I received in the past straight to you
Gmail account.

Best Regards,

Herman Pieper

On 6 apr, 14:58, "K.M Hrishikesan" <hrishik...@gmail.com> wrote:
> Hi
> Can anybody suggest a reputed supplier for RT film digitizing unit? what
> will be the approximate cost of the unit?
>
> Thanks
> Hrishi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

To unsubscribe, reply using "remove me" as the subject.




This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it. ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it. ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it. ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...