Wednesday, April 7, 2010

Re: [MW:4740] PWHT Technician'sTraining Requirements

Subramani,

I have dealt with a lot of PWHT guys down the years, there doesn't
appear to be any formal system of qualification. The majority of them I
know are however trained electricians and the rest just have on the job
training......

Declan

On 07/04/2010 09:03, subramak@batelco.com.bh wrote:
> Is there any reference specifications/standards or guidelines related to
> training and qualifying PWHT technicians.In the absence of above how to
> document their training/qualifications.
>
> Subramani.
>
> --------------------------------------------------------------------
> mail2web - Check your email from the web at
> http://link.mail2web.com/mail2web
>
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

To unsubscribe, reply using "remove me" as the subject.