Wednesday, April 7, 2010

RE: [MW:4734] Qualification range - AWS D1.1

Thanks, Karthik.
Now, could you please give me a Code ref for this info? We always need to back what we say up with Code ref. 
Appreciate your time and efforts,
S Vagal

--- On Wed, 7/4/10, Karthik <karthik6684@yahoo.com> wrote:

From: Karthik <karthik6684@yahoo.com>
Subject: RE: [MW:4732] Qualification range - AWS D1.1
To: materials-welding@googlegroups.com
Date: Wednesday, 7 April, 2010, 11:30 AM

Yes can weld SMAW alone ,but the thickness shall be within the qualified Range.

Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 4/6/10, Shashank Vagal <nach_sam@yahoo.com> wrote:

From: Shashank Vagal <nach_sam@yahoo.com>
Subject: RE: [MW:4724] Qualification range - AWS D1.1
To: materials-welding@googlegroups.com
Date: Tuesday, April 6, 2010, 8:13 PM

Hi,
Sorry, the test coupon was 8"dia x 1/2" thick. My mistake. Root, HP - SMAW, Rest- FCAW.
Now, with this can the welder use SMAW alone to weld on some other joints within the Code ?
Hope I am eligible for an answer this time.
Thanks,
S Vagal


--- On Tue, 6/4/10, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
Subject: RE: [MW:4713] Qualification range - AWS D1.1
To: materials-welding@googlegroups.com
Date: Tuesday, 6 April, 2010, 9:51 AM

also note that qualification required on =>1/2" thickness pipe.

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Muhammed Ibrahim
Sent: Tuesday, April 06, 2010 12:09 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:4707] Qualification range - AWS D1.1

Hi,
 
AWS D1.1 does not restrict weld metal deposit. It restrict base metal thickness.

Regards,
Ibrahim
On 5 April 2010 17:53, Shashank Vagal <nach_sam@yahoo.com> wrote:
Hi all,
We qualified some welders to 6GR on  6" dia x 7 mm thick pipes using SMAW  for root + hp (deposited about 4 mm) followed by FCAW. Now, if we want to use these welders for full SMAW - i) Is it allowed? ii) What is the new qualification to?
S Vagal


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...