RE: [MW:4731] ER70S-3 for low temperature application

Dear Ibrahim,

 

In order to assure, each batch shall be tested for impact toughness test at MDMT in addition to test conducted during PQR qualification. In general filler metal manufacturer will satisfy the requirements of ASME Sec. II Part ‘C’. Any additional requirements shall be communicated to the manufacturer in PO itself in order to meet the testing requirements.

 

Some of the reputed manufacturers such as Lincoln, Bohler could able to meet the above requirements. Please enquire with them.

 

Regards,

 

L. Prabhu kumar,

Sr. Principal Engineer,

 

Equipments & Materials Dept.,

Saipem India Projects Limited,

Nungambakkam High Road, Chennai - 600 034, India.

Tel:+91 44 43906588, Ext.: 588, Fax:+91 44 66840345,

Mobile Ph. No.: +91 9003010978.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Muhammed Ibrahim
Sent: Tuesday, April 06, 2010 8:28 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:4725] ER70S-3 for low temperature application

 

Dear Sir,

 

UCS 67 (a) (2) says 'Weld made with filler metal shall be impact tested if base metal is excempted by UCS 66 and MDMT is colder than-29 deg.c and not colder than-48deg.c and welding consumable is classified by impact test at a temperature not warmer than the MDMT by the applicable SFA Specification is used.

 

In my case I mentioned ER 70S-3 is specified for -20 deg.C as per SFA Spec. which is warmer than the MDMT of the euipment (-46 deg C).

My query is, as stated in UCS 67 I have Impact tested the PQR at MDMT -46 and passed the test. As per the proven support of PQR can I use ER 70 S3 for -46 deg.C application without seperate batch test?.

 

Regards,

Muhammed Ibrahim PK



 

On 2 April 2010 18:13, <george.dilintas@gr.bureauveritas.com> wrote:

Then you will find your answer in USC-67.
If you do not have the code or you have interpretation problems let me know.


  From: Muhammed Ibrahim [ibratech@gmail.com]

  Sent: 02/04/2010 16:34 ZE4


  To: materials-welding@googlegroups.com
  Subject: Re: [MW:4670] ER70S-3 for low temperature application

 

Hi,

 

The code is ASME SEC. VIII Div.1.

 

Regards,

Ibrahim



 

On 2 April 2010 09:58, <george.dilintas@gr.bureauveritas.com> wrote:

Could you clarify what is the application code? Section I, section VIII-1?


  From: Muhammed Ibrahim [ibratech@gmail.com]
  Sent: 01/04/2010 18:40 ZE4

  Subject: [MW:4661] ER70S-3 for low temperature application

 

Hi members,

 

Please provide a suggestion for the following query.

 

I have qualified a PQR for GTAW+SMAW with ER70S-3 & E7018-1. The PQR is impact tested at - 46 deg C at root(GTAW) and filling (SMAW) and passed (Min. 50J energy obtained).

 

As per ASME Sec.II part C, E7018-1 will support up to - 46 Deg C, but ER70S-3 will support up to - 20 Deg.C only.

 

Since I have proven the toughness through PQR, can I use this PQR for job with impact test requirement of - 46 Deg C, even ER70S-3 does not support for this temperature as per Sec.IIC?.

 
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

 




-------------------------------------------------------------------------------------------------------------------------------------------------------------------
DISCLAIMER: The information contained in this communication is intended solely for the use of the individual or 
entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged 
information. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution 
or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If 
you have received this communication in error, please notify us immediately by responding to this email and then 
delete it from your system. Saipem India Projects Limited (SIPL) is neither liable for the proper and complete 
transmission of the information contained in this communication nor for any delay in its receipt. 
-------------------------------------------------------------------------------------------------------------------------------------------------------------------

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...