Re: [MW:4687] Difference between pipes and tubes

Pipes----- Mass Transfer only(generally---ID controlled)
Tubes----- Mass And Heat Transfer ( generally--od and thick is controlled)
do not use STT for hot and fill pass
KGP

On Sat, Apr 3, 2010 at 3:06 PM, Gulam kader <armvasi@gmail.com> wrote:
Hai all,

1.Please somebody can explain difference between pipes and tubes with some references.

2. In our project continuously getting repair ( Cold lap) in hot and fill pass. can u suggest some good way to avoid or rectify this.

material Used - CS dia 68,64 and 60"

Process : Root - STT, Other - FCAW shielding by gas ( Ar80%, CO2 20%- 48 CFH)

Filler metal for FCAW : A5.20 E71T-9M

Expecting reply as soon as possible.

Regards,

Meera

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...