Re: [MW:4676] ER70S-3 for low temperature application

yes you can apply PQR.
Once proven record is available. i think your PQR is LTC ( A333)material.
regards
N.Devan

 
On 4/1/10, Muhammed Ibrahim <ibratech@gmail.com> wrote:
Hi members,
 
Please provide a suggestion for the following query.
 
I have qualified a PQR for GTAW+SMAW with ER70S-3 & E7018-1. The PQR is impact tested at - 46 deg C at root(GTAW) and filling (SMAW) and passed (Min. 50J energy obtained).
 
As per ASME Sec.II part C, E7018-1 will support up to - 46 Deg C, but ER70S-3 will support up to - 20 Deg.C only.
 
Since I have proven the toughness through PQR, can I use this PQR for job with impact test requirement of - 46 Deg C, even ER70S-3 does not support for this temperature as per Sec.IIC?.
 
Thanks & Regards
Muhammed Ibrahim PK
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Natarajan.Devan
Senior Welding Inspector
Al Furat Petroleum Co-Syria
Syria Shell Petroleum Development
Tel: 00963 11 6182103 Res
Mobile: 00963 933052385

INDIA: 0091 9840330143 Res.
Mobile: 0091 9884745254

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...