Dear Mr Sandesh,

Only if you have the possibilty of working with chlorides (SS) and sulphides (CS). I recommend you to take a look on API RP 945, NACE MR 0175 and NACE MR 0177 rules. 


Guttemberg Souza

Em 31/03/2010 04:37, Sandesh Pandey < sandesh.pandey10@gmail.com > escreveu:
Dear All


Would you suggest Test requirements for NACE for CS or SS materials.

 
With warm regards

Sandesh Pandey

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe, reply using "remove me" as the subject.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...