Friday, April 2, 2010

Re: [MW:4669] ER70S-3 for low temperature application

Could you clarify what is the application code? Section I, section VIII-1?


  From: Muhammed Ibrahim [ibratech@gmail.com]
  Sent: 01/04/2010 18:40 ZE4
  To: materials-welding@googlegroups.com
  Subject: [MW:4661] ER70S-3 for low temperature application


Hi members,
 
Please provide a suggestion for the following query.
 
I have qualified a PQR for GTAW+SMAW with ER70S-3 & E7018-1. The PQR is impact tested at - 46 deg C at root(GTAW) and filling (SMAW) and passed (Min. 50J energy obtained).
 
As per ASME Sec.II part C, E7018-1 will support up to - 46 Deg C, but ER70S-3 will support up to - 20 Deg.C only.
 
Since I have proven the toughness through PQR, can I use this PQR for job with impact test requirement of - 46 Deg C, even ER70S-3 does not support for this temperature as per Sec.IIC?.
 
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...