Tuesday, April 20, 2010

[MW:4900] PQR position qualified

Members,

In AWS D1.1, table 4.6 point 6 states that: A 3G vertical up test
qualifies for all positons. If our PQR testing includes CVN
requirement, can we go for only 3G vertical test coupon qualifying all
positons?
Please clarify.

Regards
Avinash

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Subscription settings: http://groups.google.com/group/materials-welding/subscribe?hl=en

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...