Dear All,
Please clarify below points.
The designed thickness for a plate to plate welding is 10 mm and actual thickness used in the production is 12 mm. welding requires Single side full penetration weld.
1) considering the above case is it acceptable if welding groove is filled upto 10 mm thickness only considering complete penetration on root side.
2) Is it acceptable if complete 12 mm thk groove is filled and we have incomplete penetrartion of 2 mm on root side.
Please give Code reference(if any).
Thanks & Regards
Asad Azmi