[MW:977] Re: Root under cut

Root undercut is end result of high Current, travel speed, uneven root gap and some time because of surface tension of the material and last but not least because of welder human error. To avoid under cut mainly focus should be given on current and travel speed. Undercut problems are not envisaged with cellulose electrode if proper welding parameter set along with good skill welder. Some time re shuffling of root welders also help to reduce down root related discontinuities.
 
Regards
 
Paresh

 
On 7/28/08, atul patil <atulpatil99@gmail.com> wrote:
to avoid root undercut
thanks in advance

 
On 7/27/08, Paresh Katvi <pkatvi@gmail.com> wrote:
Dear Atul
 
Ar you looking for information How to avoid root undercut or NDT method to analisied under cut in most sensitive manner?
 
please give further information.
 
Regards
 
Paresh Katvi

 
On 7/22/08, atul patil <atulpatil99@gmail.com> wrote:
Dear all
I am working with Gas export pieline in Kazakhstan
We are using 6010 electrode for root
& 8010 for fill cap
 
we are facing the problem with root undercut
 
Actually on the basis of radiography ( ISO 13847 ) doesnt ask to cmpareason of density with parent metal It says only about length
 
Please guide
It is very difficult to prepare the calibration block for UT ( Manual ) in my city ( Atyrau )
Could you please guide
any  suggestions welcome.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...