Friday, July 18, 2008

[MW:945] RE: 944] Suitable electrodes for Duplex Stainless steel (UNS S31803)to Copper Nickel alloy (Cu70Ni30)

Thou’ I have not tried anytime, recommended filler for copper to steel is ERCuAl-A2 (note that the selection is based on weldability, and not for mechanical strength), give a try with this

Adequate preheat and inter pass temp, based on thickness / joint configuration, Helium or argon/helium mixture would give better results.

 

Do remembers to update members here with your results.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mathu.subramanian
Sent: Thursday, July 17, 2008 5:24 PM
To: materials-welding@googlegroups.com
Subject: [MW:944] Suitable electrodes for Duplex Stainless steel (UNS S31803)to Copper Nickel alloy (Cu70Ni30)

 

Dear Friends,

 

Can u please suggest Suitable electrodes for Duplex Stainless steel (UNS S31803) to Copper Nickel alloy (Cu70Ni30).

 

Regards,

 

S.Mathusoothanan


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...