Hi Nilesh,
 
Since the casing is carbon steel base material, so due to caustic service their is a possibility of "Caustic Stress corrosion cracking" when temp is about 80 Deg C, and due to its inherent stresses..
 
Thanks and regards,
 
Venugopal
Singapore
============================
 
 


 
On Thu, Jul 17, 2008 at 1:05 PM, Darji Nilesh (Mumbai - Machinery) <N.Darji@ticb.com> wrote:

In Process data sheet, Process has asked to perform PWHT for Centrifugal pump Material due to caustic service.

 

Pump casing material is A 216 Gr WCB.

 

Can any one clarify why It is required !! any specific reason !!

 

Regards,

 

Nilesh.





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...