[MW:936] RE: 933] PWHT - Caustic service

At temperatures above ambient, corrosion rates of carbon steel become greater and is accompanied by a risk of caustic stress corrosion cracking (CSCC). Low concentrations of caustic can be safely handled by carbon steel up to 180oF/82oC, where CSCC starts to become a risk factor, while the safe upper limit for a 50% solution is approximately 150oF/65oC, although cracking has occurred at temperatures as low as 120oF/48oC. The Caustic Soda Service Graph (attached pic) is a widely used guide for determining safe operating temperatures with respect CSCC of carbon steels at various concentrations of caustic.

 

Conclusion: PWHT generally recommended by process designer for CS used caustic service, mainly based on two parameters, concentration of the solution and operating temperature.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Darji Nilesh (Mumbai - Machinery)
Sent: Thursday, July 17, 2008 10:36 AM
To: materials-welding@googlegroups.com; Pressure_Vessel@yahoogroups.com
Subject: [MW:933] PWHT - Caustic service

 

In Process data sheet, Process has asked to perform PWHT for Centrifugal pump Material due to caustic service.

 

Pump casing material is A 216 Gr WCB.

 

Can any one clarify why It is required !! any specific reason !!

 

Regards,

 

Nilesh.



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...