Tuesday, July 15, 2008

[MW:928] PWHT of SA 333 Gr.3


Dear Friends,
 
I encountered a problem with SA333 Gr.3 (P9B) material PWHT. The material is quenched and tempered. As per ASME SEC II the tempering temperature of this material is  565-605 degree celcius. But ASME B31.3 allows the PWHT 593-635 degree celcius.

 Is it allowed to do so? Will it effect the tempering property of material if it do above the tempering temperature?


Thanks & Regards
Muhammed Ibrahim PK

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---