No requirements as such in the code, only thumb rules or from contract specifications

One of them is (rather easy to remember)

Minimum distance between two welds =   (where ‘D’ is OD of pipe and ‘t’ is wall thickness in mm)

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of john saji
Sent: Wednesday, July 02, 2008 1:10 PM
To: materials-welding@googlegroups.com
Subject: [MW:890] weld distance

 

Dear members

coudl you please expain what is the minimum distance(toe to toe) between butt weld and fillet weld AS PER B31.3?

 

GIFTO599 VINCOTTE




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...