We have to weld a Baffle plate of 10mm Thick inside an EQ. TEE (24'', 36'' & 42''). The thickness of the TEE is 9.53 mm and all the EQ. TEES are welded construction with 100% RT. The Baffle plate is welded in such a way that, it will block the one run side of the EQ. TEE. Now the welding of the Baffle plate, will it creates and problem as it intersect with EQ. TEE weld at some point. Can we have two welding at a same point? The Baffle plate is fillet welded. The working pressure is 1 bar.
Kindly advice me,
Thank you,
Regards,
Sabir
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Monday, July 14, 2008
[MW:920] Re: Welding Baffle Plate on EQ. TEE
Dear Zameer
As per sec VIII u can welld over weld. dont worry u can weld ir , but do 100% MPI or DP
Regards
Shabbir
On 7/13/08, Zameer Mohammed <dreamthinkwork@gmail.com> wrote:
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...