[MW:903] UG 20(f) - Clarification

For thickness above 25mm, you need to refer UCS 66 for a combination of material grade and thickness and MDMT, please refer UCS 66(a)

UG20 (f) is referred from UCS 66(a), not vice versa, and UG20 (f) exemption can be taken when all of the condition given are met.

 

In your case 516 Gr70N, refer curve D in fig UCS 66 against MDMT and thickness, for e.g. if your MDMT is not colder than -29 °C, CVN impact may be exempted up to 1.25 inch in thickness

 


From: Pressure_Vessel@yahoogroups.com [mailto:Pressure_Vessel@yahoogroups.com] On Behalf Of GIRISH KUMAR
Sent: Saturday, July 05, 2008 8:05 PM
To: Pressure_Vessel@yahoogroups.com
Subject: RE: [Pressure Vessel] Clarification

 

material is a516 GR.70 normalised when i refered the fig ucs 66 the impact test doesn't need if i go to UG 20f it required I have the only one clarification is which we take as final. because ug 20f clearly says the material p1 group thickness exceed 25mm require impact test

--- On Sat, 7/5/08, amol gengaje <amolgengaje@yahoo.co.in> wrote:

__._,_.___


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...