[MW:900] Re: pre heat for dissimilar metals

Dear Ibrahim,
 
Standard also ask to follow ASME SEC IX for Welding process & qualification. Finally pupose of all std soundness of welding joint.
 
Regarding your query abour the preheat . There is not mandotory requirments of preheat temaprature for CS to SS weld for thicknes up to 2 1/2'' but you can preheat up to 60'c good practioce for welding what we are using.
 
Thanks,
 
Vikas Rana

 
On 7/3/08, Muhammed Ibrahim <ibratech@gmail.com> wrote:
Any body can help me to decide the pre heat temperature for welding of carbonsteel with stainless steel?  If thickness is greater than 32mm,  preheat is mandatory in SEC VIII. But in this case what I can follow. Carbon steel preheat temperature or stainless steel preheat temperature?.
If it damage the property of stainless steel is it mandatory?

Thanks & Regards
Muhammed Ibrahim PK
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...