Pre heat only on CS side
From:
Sent: Thursday, July 03, 2008 7:14 PM
To:
Subject: [MW:893] pre heat for dissimilar metals
Any body can help me to decide the pre heat temperature for welding of carbonsteel with stainless steel? If thickness is greater than 32mm, preheat is mandatory in SEC VIII. But in this case what I can follow. Carbon steel preheat temperature or stainless steel preheat temperature?.
If it damage the property of stainless steel is it mandatory?
Thanks & Regards
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---