Wednesday, July 2, 2008

[MW:889] RE: 888] %RT on nozzle long seam per API650

Dear Raghuram,

 

Please note that the clause 5.7.8.11 is only applicable to flush type connection. (Pl. start reading from 5.7.8)

 

Regards,

 

S.Mathusoothanan

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: 02 July, 2008 2:02 PM
To: materials-welding@googlegroups.com
Subject: [MW:888] %RT on nozzle long seam per API650

 

Ref: API650 2007 edition

 

Para 5.7.8.11 states ‘All longitudinal butt-welds in the nozzle neck etc…………..shall receive 100% radiographic examination (see 8.1)

Where as in para 8.1.1 states ‘Radiographic inspection is not required for the following:…………welds in nozzle and man way necks made from plate’

 

Which one is correct or am I not interpreting correctly?

 

Note: if you are referring old editions it is same (just refer para 3.7.8.11 and 6.1.1 instead of the above)



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...