Monday, April 5, 2010

[MW:4691] What is filler metal for GTAW process for A240 - 321 to A266

Dear all
What is the filler metal for GTAW process when welding A240 - 321
plate with A266 Gr 1 Tube sheet forging?
--
Regards,
Rupesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

To unsubscribe, reply using "remove me" as the subject.

1 comment:

Ashfaq Anwer said...

You may use either ER309 or ERNiCr-3.

Hope this would help.

Regards,
Ashfaq Anwer
http://forums.thepetrostreet.com