Re: [MW:24409] Welding by SAW process is it mandatory for heavy thick vessels in H2 service

You may use SMAW with approved WPS and with expert welder but, as compared to SAW the productivity is too less, chances of defects are more, more workmanship required, more precise testing is required and no client will take chance for the delay and the quality. 

Regards,

Anosh Wankhade




From: Kannayeram Gnanapandithan <kgpandithan@gmail.com>
Sent: Mon, 29 Feb 2016 11:10:12
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:24404] Welding by SAW process is it mandatory for heavy thick vessels in H2 service
SMAW is a time consuming and quality purely based on welder skill. SAW process is also available in Semi-Automatic process, it is gives better quality of weld, fast, aesthetic look

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Sat, Feb 27, 2016 at 9:12 PM, <dilintas@gmail.com> wrote:
Almost 20 years ago I was in a tank farm project were field welds were performed by means of saw

Sent from my BlackBerry 10 smartphone.
From: Prasad
Sent: Σάββατο, 27 Φεβρουαρίου 2016 - 09:02
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:24384] Welding by SAW process is it mandatory for heavy thick vessels in H2 service

Dear welding experts,

We are manufacturing heavy wall vessels for H2 service.
MOC SA 516 Gr 70. Thick 56 mm
Due to large size vessels are to be supplied in two sections.
Hence on site weld joint will have to be done at place of installation.
At shop we are using SAW process for welding.
At field rotating is not possible and we want to use SMAW process.
Our client is asking us to use SAW process for field weld joint also.

We know that SAW is semi automatic & more productive process.

My question is whether is their any restriction to use SMAW process.

Request experts to give their valuable views to convience client technically.

Best regards,

Prasad Ghanekar


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb19d5b1-6c54-45fe-8e91-1346dd8c9617%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160227154234.6713426.85120.1966%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMGZGYtAK5gG1pnsB4W2OZ9KngLfpg5Mn4_MM1Nib1tGQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1456724412.S.18199.30999.f6-235-206.1456734926.27074%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...