Hi,

Level 3 certification in PAUT, TOFD, etc is issued by PCN BiNDT. There are Level 3's in these techniques.

Sent from my iPad

On 17-Feb-2016, at 11:35, 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Hi,
PAUT, TOFD, etc are the techniques of UT method. If you have a Level III in UT, you may go for additional training for these techniques and be a so-called specialist. But mere training and certification may not make you competent, so to say to do justice to the job. You will master these techniques only by on the job experience by lot of practice on different types of test specimens.  
As such there is no specific Level III in this technique, but a UT Level III is qualified to write / review these procedures and a well experienced Level II individual can do the actual job. If required, the client may test him on a mock up test piece. This is the industry practice.
 
BR,
Shashank C Vagal 



From: pgoswami <pgoswami@quickclic.net>
To: materials-welding@googlegroups.com
Sent: Wednesday, 17 February 2016 5:08 AM
Subject: [MW:24310] RE: 24309] PAUT & TOFD Level III

Hi Mostafa,
 
These techniques are very specialized techniques. Not all NDE techs are up to speed with both of these techniques. Please see some guidelines from the BINDT on the same.
 
I'm not sure , where you're located, you may check with the local high profile NDE Schools or Companies, who'll have those personnel in their team
 
Thanks.
 
 
Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist & Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]
Sent: Tuesday, February 16, 2016 8:25 AM
To: Materials & Welding
Subject: [MW:24309] PAUT & TOFD Level III
 
Dear Sir,
Kindly clarify if  there is level III in PAUT&TOFD or not. our client insists for level III in PAUT&TOFD for PAUT procedure review and level II in PAUT&TOFD to carry out the work. i searched many but i found NO body has this certificates. are these certificates true? and how can i get it?
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/855091088.3944591.1455629104764.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAI6C/nhitp9NlnqAyYQt%2BycBAAAAAA%3D%3D%40quickclic.net.

For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1141766489.4415183.1455694544189.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...