Skip to main content

Re: [MW:24368] Flange Buttering

I would help if you send a drawing or a sketch

Sent from my BlackBerry 10 smartphone.
From: sankar bombay
Sent: Πέμπτη, 25 Φεβρουαρίου 2016 - 05:37
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: Re: [MW:24366] Flange Buttering

It's for butt joint what about flange inside buttering to reduce gap between pipe and flange (slip on flange ) ... 

There is any heat treatment required for flanges 

Thanks for your reply

Best regards
Sankar

On Tuesday, February 23, 2016, Jim Price <JimPrice@polarcorp.com> wrote:

 

Please see UW 42 of ASME Section VIII Div 1.  A butt welding procedure is enough for buttering.

 

UW-42 SURFACE WELD METAL BUILDUP
Construction in which deposits of weld metal are applied to the surface of base metal for the purpose of:
(a) restoring the thickness of the base metal for strength consideration; or
(b) modifying the configuration of weld joints in order to provide the tapered transition requirements of UW-9(c)
and UW-33(b) shall be performed in accordance with the following rules:
(1) A butt welding procedure qualification in accordance with provisions of Section IX must be performed for
the thickness of weld metal deposited, prior to production welding.
(2) All weld metal buildup must be examined over the full surface of the deposit by either magnetic particle
examination to the requirements of Appendix 6, or by liquid penetrant examination to the requirements of Appendix 8.
When such surface weld metal buildup is used in welded joints which require full or spot radiographic examination,
the weld metal buildup shall be included in the examination.

 

Reference Appendix 6 Section VIII Div 1

Buildup QW202.3

Thickness QW451.1

 

Best Regards

 

 

Jim Price | Welding Engineer, CWI

Direct:  320.7463439 | Fax: 417-862-5564

jimprice@polarcorp.com

cid:image001.jpg@01D0E005.E9837830

 

 

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sankar krishnan
Sent: Monday, February 22, 2016 11:38 PM
To: Materials & Welding
Subject: [MW:24361] Flange Buttering

 

Dear All,

 

   In my project Slip on flange to Pipe We have 7 mm gap .. Pipe have ovality 

 

Now my client saying to us to do buttering at flange at machining 

 

If we do buttering at flange its allowed in the code book 

 

Please guide me

 

Best regards

Sankar.k

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/97c5d7b8-713a-4625-afc8-9bcbd722e7a2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/384a8124d1864f99b29e940c10997808%40POLARMAIL.PolarTank.local.
For more options, visit https://groups.google.com/d/optout.


--
shankar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyDEeYkrrG%3D7_t3_hRjG6K9aPz1WC-Te-F85ZHbvwVfESPiAg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...